Nanocrystalline or Ferrite for SST High-Frequency Transformers? Analyzing Loss, Temperature Rise and Cost from Winding Turns
Core Conclusion
Nanocrystalline materials allow higher operating flux density to reduce winding turns. However, fewer turns do not automatically mean the transformer is more efficient, runs cooler or costs less. It is necessary to calculate core loss, copper loss, insulation and thermal dissipation costs simultaneously.
For projects with loose dimensional constraints, prioritizing cost and manufacturing repeatability, it is recommended to evaluate mature ferrite solutions first. For applications with strict requirements on volume, weight or window utilization, nanocrystalline cores should be assessed intensively. This guidance defines an engineering evaluation sequence and cannot replace specific grade selection and prototype testing.
This article discusses general trade-offs between materials and structures. No proprietary design parameters for specific projects are disclosed. N and N/2 used herein are for illustration only; such comparison does not guarantee identical benefits for any pair of materials.
1. Clarify the Comparison Scope
High-frequency transformers inside SSTs deliver power transfer and galvanic isolation. Material selection must be benchmarked under identical output capacity, operating frequency, cooling conditions and insulation acceptance criteria.
Datasheets from core manufacturers show that nanocrystalline materials feature high saturation flux density, while power ferrites have a well-established high-frequency application ecosystem [1][2]. Saturation flux density, nevertheless, is not the allowable operating flux density. The actual operating point is determined by frequency, waveform, temperature and acceptable loss budget.
Before comparison, obtain loss curves of candidate grades and unify temperature and waveform conditions. Normalize loss metrics (W/kg and kW/m³) to the same basis and convert them into total loss of the complete core.
2. Why Can Nanocrystalline Cores Potentially Reduce Winding Turns?
For symmetric bipolar square waves, the preliminary relationship is:
N ≈ V / (4fAeBpk)
Where:
N = number of winding turns; V = amplitude of square-wave voltage across the excitation branch; f = frequency; Ae = effective cross-sectional area; Bpk = peak flux density.
Given fixed voltage, frequency and cross-sectional area, if nanocrystalline material can operate at roughly double the flux density within acceptable loss and temperature rise limits, the required turn count can drop from N to approximately N/2.
Primary and secondary turns shall be adjusted proportionally to maintain the defined turns ratio. The comparison targets feasible operating points, rather than simply dividing the saturation flux density of the two materials.
| Winding Turns & Material Utilization | |
|---|---|
| Ferrite | When operated at relatively low flux density, more turns or larger conductor cross-section are generally required. |
| Nanocrystalline | Higher allowable operating flux density creates opportunities to reduce turns or conductor size. The two benefits cannot be maximized simultaneously. |
3. Performance Changes After Reducing Turns
3.1 DC Resistance: Potential Reduction
If average turn length, conductor cross-section and temperature stay unchanged, conductor length scales with turn count. When turns are cut from N to N/2, winding DCR can be roughly halved. In practice, terminals, connection segments and lead wires will not shrink proportionally.
3.2 Copper Loss: AC Resistance Matters More Than DCR
Assuming identical RMS current and AC resistance factor, halved DCR approximately halves the corresponding copper loss. However, changes in winding layers, magnetic field distribution and current sharing will alter proximity effect. Cutting turns in half does not guarantee AC copper loss is also halved.
3.3 Core Loss: Higher Flux Density Comes With a Penalty
Fewer turns raise operating flux density. Even without saturation, core loss may increase significantly. Engineers must verify whether saved copper loss outweighs incremental core loss and additional parasitic losses; copper savings alone are insufficient for judgment.
3.4 Inter-turn Insulation: Higher Voltage Per Turn
With total winding voltage unchanged, halving the turn count roughly doubles the average voltage across each turn. End electric field, sectional winding layout and lead routing need redesign. Primary-to-secondary main insulation cannot be thinned automatically with fewer turns.
3.5 Inductance and Parasitics: Original Structure Cannot Be Reused Directly
Under fixed magnetic circuit conditions, magnetizing inductance scales with the square of turn count. Effective permeability also shifts after material replacement. Leakage inductance depends on turns and winding geometry, while parasitic capacitance relates to overlapping area, clearance and connection scheme. All these parameters require recalculation and testing.
3.6 Window Utilization: Space Saving May Be Offset by Insulation
Fewer turns help reduce copper occupation, winding layers and labor hours. Yet higher voltage per turn, end clearances, insulation barriers and thermal channels may consume part of the space gain.
4. Fair Comparison of Loss and Efficiency
Comparison formula:
Total Loss = Core Loss + Winding Loss + Additional Loss (dielectric loss, shielding loss, etc.)
For the same output power, transformer efficiency η = Pout / (Pout + Total Loss). Transformer efficiency should not be confused with the efficiency of the whole converter.
Nanocrystalline cores deliver a loss advantage only when:
Incremental core & additional loss of nanocrystalline < Copper loss saved by reduced turns.
If this condition fails, a design with fewer turns may end up with lower efficiency.
The following dimensionless loss index demonstrates this rule. Take ferrite as baseline with total loss = 100 (copper loss 40, core loss 50, other loss 10):
| Case | Description | Total Loss |
|---|---|---|
| Baseline (Ferrite) | Copper 40 + Core 50 + Other 10 | 100 |
| Case A (Nanocrystalline) | Copper 20 + Core 60 + Other 10 (copper savings exceed incremental core loss) | 90 (10% lower) |
| Case B (Nanocrystalline) | Copper 20 + Core 90 + Other 10 (incremental core loss cancels copper savings) | 120 (20% higher) |
These are purely arithmetic illustrations, not material datasheet values, simulation outputs or prototype test results. A 10% reduction in total loss does not equal a 10 percentage-point efficiency gain; efficiency improvement depends on the ratio of loss to input power.
5. Temperature Rise, Volume and Cost Trade-offs
5.1 Hotspot & Temperature Rise
Ferrite: Multi-turn windings tend to generate higher copper loss. Hotspots inside coils and at wire outlets need careful inspection.
Nanocrystalline: Fewer turns may ease winding heating, but elevated flux density can increase core heating. Total loss alone cannot determine the critical hotspot.
Temperature rise is affected by both loss and thermal resistance. Lower loss helps reduce overall temperature only under identical cooling conditions. Separate thermal paths should be established for windings and cores, with measurements taken under actual cooling schemes.
5.2 Volume & Weight
Ferrite: Standardized cores are easy to configure. Larger window and main insulation space requirements mean more turns do not necessarily make the finished product unacceptably bulky.
Nanocrystalline: Higher flux density can optimize core or winding size. The density of metallic nanocrystalline ribbons and required insulation protection must be included in weight calculation; bare core volume comparison is inadequate.
5.3 Manufacturing & Processing
Ferrite: Mature cores, bobbins and winding processes are preferred. Evaluate winding layers and assembly of stacked cores.
Nanocrystalline: Assess risks introduced by ribbon cutting, joint interfaces, mechanical stress, protection and potting. Do not assume processed cores retain the original material performance.
5.4 Total Cost
Ferrite: Standardized supply chains often bring advantages in cost and lead time, subject to formal quotation and yield data.
Nanocrystalline: Savings on copper material and winding labor may be offset by core machining, protection and validation expenses. Full lifecycle cost of the finished assembly must be calculated.
Quotation scope shall uniformly cover cores, copper, insulation parts, resin, assembly, thermal management, testing, rework and scrap. Amortized development cost, order quantity and alternative supply capacity should also be considered. Fixed price gaps shall not be stated without formal quotes.
6. Epoxy Potting Insulation: Why Core Size Alone Is Not Enough
High-voltage isolation transformers reserve dedicated space for primary-secondary main insulation, end clearances, lead outlets and thermal channels. Reduced winding turns do not allow proportional shrinkage of these spaces.
Main insulation thickness refers to the thinnest continuous effective dielectric path between primary and secondary windings. Actual thickness is determined collectively by test voltage, waveform, dielectric system, interface condition and end electric field, and cannot be directly derived from the short-term breakdown strength of epoxy resin.
In a simplified single homogeneous dielectric model, average electric field roughly equals voltage divided by thickness. In real structures, corners and end regions create concentrated local electric field, and voltage redistributes across multiple dielectric media. Electric field simulation based on real geometry and material parameters is required instead of a universal “mm per kV” rule.
Epoxy potting needs strict control of material drying, impregnation, degassing and curing. Voids, cracks and interfacial delamination must be checked. OMICRON documents note such defects can trigger local field concentration and partial discharge [4]. Thicker resin cannot substitute robust process control.
Ferrite and nanocrystalline designs must meet identical insulation acceptance criteria before structural comparison. Space saved from smaller windings may be consumed by main insulation and end optimization. Increased potting thickness also changes thermal resistance, average turn length and leakage inductance.
Engineering recommendation: validate insulation coupons first, then full prototypes. Evaluate withstand voltage, partial discharge and performance after thermal cycling separately. Test thresholds, insulation thickness and potting formulation for internal projects are not disclosed here.
7. Final Guidance: Start With Ferrite, When to Switch to Nanocrystalline?
Prioritize ferrite when dimensional margin is sufficient, and cost & manufacturing stability are top priorities. Ferrite serves as a benchmark for manufacturing and cost; this does not mean ferrite delivers the lowest loss under all operating conditions.
Evaluate nanocrystalline intensively when ferrite hits limits on window space, volume, weight or loss. Nanocrystalline becomes the preferred option only when copper loss and space benefits from reduced turns outweigh incremental core loss and manufacturing overhead, and verified under identical test conditions.
Material upgrade shall satisfy three criteria: net gain in total loss, tangible improvement of finished structure, and acceptable overall cost. Insulation reliability is a mandatory threshold for both solutions.
8. Frequently Asked Questions
Q1: Are nanocrystalline cores always more efficient than ferrite? No. Efficiency advantage exists only when total loss is lower. High saturation flux density and fewer turns are not standalone proof of higher efficiency.
Q2: Can copper loss be halved if turns are cut in half? Approximate estimation holds only when average turn length, conductor cross-section, current, temperature and AC resistance factor remain consistent. AC loss shall be recalculated after structural modification.
Q3: Will temperature rise definitely drop with fewer turns? Not necessarily. The winding may run cooler while the core becomes hotter. Hotspots of core, winding and leads should be checked separately.
Q4: Can I reuse the original winding after switching core material? Direct replacement is not recommended. Recheck flux density, inductance, leakage inductance, parasitic capacitance, soft-switch compatibility and insulation layout, then verify system operation.
Q5: Will high-voltage insulation requirements change material selection? Yes. Main insulation and end clearances often define overall product size. Meanwhile, electric field control and process management are required for the sharp edges of metallic nanocrystalline ribbons, ferrite surfaces and all material interfaces. Passing hipot test does not replace partial discharge validation.
Q6: How to make the final decision? Compare total loss, hotspots, form factor, weight, quotation and manufacturing consistency of two prototype sets under identical operating, insulation and cooling conditions. Establish the baseline with ferrite first. Switch to nanocrystalline only when the full finished product demonstrates clear benefits.
Q7: Can primary-secondary epoxy potting insulation be designed to a fixed thickness? No. Thickness is determined by test specification, resin & interface property, end electric field and manufacturing process. Dielectric breakdown strength cannot be directly treated as the allowable field strength free of partial discharge. Proper thickness does not exempt partial discharge and thermal cycling validation.
Q8: Is thicker primary-secondary insulation always better? No. Extra thickness may reduce field stress in certain regions, yet occupies window space, raises average turn length and thermal resistance, and modifies leakage inductance. Loss, temperature rise and dimension shall be co-optimized under verified electric field and insulation performance.
Closing Remarks
The core of material selection for high-power transformers is whether the whole system performs better after reducing winding turns. Ferrite is suitable for building a proven baseline scheme, while nanocrystalline is adopted to capture performance gains under hard constraints. The final judgment depends on finished loss, temperature rise, insulation reliability and total cost, not the material name itself.
YEH-TEK
We specialize in flat wire inductors, planar transformers and high power density magnetic components. We provide collaborative optimization covering core material, magnetic circuit, winding and thermal design, delivering magnetic component design and manufacturing solutions for AI power supplies, AIDC, energy storage and high-power DC-DC applications.
References
[1] VACUUMSCHMELZE, Nanocrystalline Cores for Medium-Frequency and Solid-State Transformers, April 2025. Scope cited: material characteristics of nanocrystalline cores for MF and SST transformers; no finished product performance is inferred hereby. https://vacuumschmelze.com/03_Documents/Brochures/Product%20Information%20Nanocrystalline%20Cores%20for%20MF%20and%20SSt.pdf
[2] TDK Electronics, Ferrites and accessories — SIFERRIT material N87, June 2025. Scope cited: power ferrite material parameters and loss variation against operating conditions. https://www.tdk-electronics.tdk.com/blob/528882/download/3/pdf-n87.pdf
[3] Texas Instruments, Planar Transformers, Technical Document. Scope cited: trade-offs among winding structure, high-frequency copper loss and thermal design. https://e2e.ti.com/cfs-file/__key/communityserver-discussions-components-files/196/planar-transformers.pdf
[4] OMICRON, What is Partial Discharge?, 2020. Scope cited: insulation defects, voids and local electric field; no universal qualified thickness is derived from this document. https://www.omicronenergy.com/download/document/DC269570-F045-46A0-845A-CFF654BBEDDE/